Now you can repair aluminum and zinc based parts with out a welding machine :

  • All you need is a hand held propane type torch for small pieces.
  • Produces a sound joint that is stronger than the parent metal.
  • No fluxes are required.
  • There are no fumes.
  • Low 732°F. working temperature.
  • Joins thin or thick parts

Try the difference between hts-2000, Alumaweld, Alumarod, Alumaloy, A-LUM-RITE by Divesco, Aladdin 3 in 1 or hts2000 :
Durafix EASYWELD is the best !

Use DURA-FIX For : INDUSTRIAL MAINTAINANCE - FABRICATE REPAIR - FARICATION MAINTAIN - ALUMINUM AND ALLOY

BOAT OWNERS / ARTISTS / HOBBYISTS / RADIATOR SHOPS / VOCATIONAL SCHOOLS /RACE CAR MECHANICS / LOCKSMITHS / GO-CART RACERS / CAMPING ENTHUSIASTS / PLUMBERS / WELDERS / FARMERS / FISHERMEN / HUNTERS / GUNSMITHS / AVIATORS / SPORTSMEN / MACHINISTS / AIR CONDITIONER REPAIRMEN / LAWNMOWER REPAIR SHOPS / TRANSMISSION REPAIRMEN / MOTORCYCLE REPAIRMEN / AUTO-BODY REPAIRMEN / MAINTENENCE MECHANICS / STORM WINDOW FABRICATORS / SOLAR ENERGY FARICATORS / ANTIQUE CAR RESTORATION / And many more...

aluminum welding rodsFEATURES :

  • LOW COST
  • STRONGER THAN ALUMINUM
  • NO FLUXES OR FUMES
  • LOW WORKING TEMPERATURE

Aluminum Welding Instructions :

If you have any problems with Durafix EASYWELD or any questions, do not hesitate to contact us. We will give you personal instructions on how to use our product. Customers that call us with problems leave very satisfied and usually order again.

Clean area to be welded down to base. Brush the base with stainless steel brush till shiny. Heat the area to be welded, evenly. As you heat the base, rub the rod vigorously against the heated piece to be welded till rod flows. Never apply heat directly to rod.

security :

ALWAYS WEAR SAFETY GLASSES AND GLOVES !

Do not use on magnesium.

If you are unsure of the the material, file off some metal and apply the torch. Magnesium will burn white like a flare.
Will not be held liable for any damages, injury or losses due to the misapplication of this product or any other reason whatsoever

Download Technical specifications :

Product Description
Technical details
Technical details 2

 

NOW WELDING ALUMINUM IS AS EASY AS 1 - 2 - 3

altaltalt

HOW TO WELD ZINC BASED METALS WITH Durafix EASYWELD ROD

alt alt alt

Vee the broken edges to about 45 degrees, clean the surface of any plating or scale back from edges of the vee 1/8 of an inch.

Heat until it starts to flow. Turn flame paralell to surface and with side of flame, hold at this heat. Heat welding rod to same temperature. Now with both bases and welding rod at this temperature, touch rod to the break and rod will flow into vee, thoroughly fusing the parts.

Repeat operation until break is completely filled. Be sure to kick rod into weld to break down skin resistance as filler rod will lay on surface and will not fuse if only heat is applied.

HOW TO REPAIR A PROPELLER

alt

alt

alt

alt

Wire brush throughly to break up surface oxide and remove paint.
Heat hot enough to flow rod without the aid of the flame. Tin the flat (not beveled) side and attach a temporary support of carbon or copper.
Turn and tin beveled side, building out the blade slightly larger than its original size. Grind damaged edges to a 45 bevel. Pitch propeller to standards.
Let cool, then grind to proper standards. Results? ... a well prepared wheel without porosity for you to balance and paint!

Specifications :

Tensile Strength,lbs/sq. in. :
Compression Strength,lbs/sq. in. :
Shear Strength,lbs/sq. in. :
Charpy Impact Str,lbs/sq. in. :
Hardness (Brinell) :
Ductility Good :
Melting Point :
Specific Gravity :
Density (Ibs/cu. in.) :
Elongation (in 2") :
Coefficient of Linear Expansion :
Electrical Conductivity :
Thermal Conductivity :
Dimensions :

47,000
60,000 - 75,000
34,000
4 ft/lb to break 1/4" bar
100
Good
732°F/390°C
6.7
0.25
3%
15.4x10-6/°F
24.9% du Cu
0.24 cal/cu. cm/°C
L : 45cm / Ø 3.2mm

Dura-FIX Rod

The most widely used rod on the market for WELDING ZINC BASE metals - white - die cast - pot metal. Alloyed from pure virgin metals. Welds made with ROD are clean and free from slag. Produces a sound joint that is stronger than the parent metal. BRAZING ALUMINUM without the use of flux, sound and free from porosity. SOLDERS GALVANIZED, also used as a RUB-ON solder. Use a slightly carburizing flame (excess of acetylene), with small tip for most work. MELTING POINT 732°F. Dura-Fix Is Used TO: Repair Kirksite dies, power tools, aluminum radiators, power mower castings, propellers, lower units and boat hulls. THOUSANDS OF OTHER USES.

General Notes

This rod will work with propane, mapp, butane, oxyacetylene or any fuel source as long as the material is brought up to 732°F. The rod will not work if heated directly. You must heat the material that you are working on to 732°F and then apply the rod. The material must be cleaned with a stainless steel brush (included) because the rod will not adhere to stainless steel. The rod will not adhere to the material being brazed if it is cleaned with a steel or other type brush.

Exemples in video :

Order online :

www.1001discount.com

To contact us : contact@durafix-easyweld.com